[SEM18-09] Experimental evaluation of remanence carriers in coercivity-blocking temperature diagram

*佐藤 雅彦1寺田 卓馬2望月 伸竜3伊藤 理子2綱川 秀夫2 (1.東京大学、2.東京工業大学、3.熊本大学)

キーワード:Anhysteretic remanent magnetization、Coercivity、Blocking temperature、Paleointensity

Knowledge of the remanence carrier in recording media is crucial for obtaining reliable paleomagnetic data. Here we report newly developed technique to evaluate the remanence carrier of natural rock samples using anhysteretic remanent magnetization (ARM) spectra in coercivity (Hc) and blocking temperature (TB) plane (hereafter referred to as Hc-TBdiagram). Experimental procedures are as follows: (1) imparting ARM at 50 μT DC field and 140 mT AC field, (2) thermal demagnetization (THD) for the ARM at a certain temperature, (3) stepwise alternating field demagnetization (AFD) for the remaining ARM, (4) repeating steps 1–3 with THD treatment at a higher temperature, and (5) calculating second derivative of ARM on the Hc-TBplane. Samples from three basaltic lavas and two welded tuffs were used for Hc-TBdiagram experiments. The basaltic lava samples consist of HW95 from Hawaiian 1995 lava flow of pahoehoe, OS86 from Izu-Oshima 1986 lava flow at the northwest flank of Mihara Volcano (Japan), and UN01 from Kiso-ontake lava flow (called Ueno basaltic rocks) in Nagano (Japan), which extruded during the Matuyama chron. The welded tuff samples were KM01 from Komagatake welded tuff and SK03 from Shikotsu welded tuff, both of which extruded 30-35 ka in Japan. In the cases of HW95, UN01, and KM01 samples, remanence carriers are composed mainly of a single phase in the Hc-TBdiagram. The OS86 sample showed two phases in the Hc-TBdiagram which can be distinguished from each other by AFD treatment but not THD treatment because of similar TBspectra. In the case of SK03 sample, second derivatives of ARM showed not only positive values but also negative values in the Hc-TBdiagram. The negative value implies significant effects of thermal alteration due to laboratory heating. On the basis of Hc-TBdiagrams, we will further discuss remanence carriers in the measured samples.