[3B12] Behavior characterization of volatile fission products in meltdown nuclear fuels by a method in consideration of surface and interface effects

(4)Effect of solid surface morphology on melting behavior of CsI

*Hiroto Ishii1, Ken Kurosaki1,2, Yukihiro Murakami3, Yuji Ohishi1, Hiroaki Muta1, Masayoshi Uno3, Shinsuke Yamanaka1,3 (1.Osaka Univ., 2.JST PRESTO, 3.Univ. of Fukui)

Keywords:Wettability,, Yttria-Stabilized Zirconia, Caesium Iodine

表面が平滑なイットリア安定化ジルコニア(YSZ)の単結晶基板上と、表面に粗さを有するYSZ多結晶体上のそれぞれで、ヨウ化セシウム(CsI)の溶融試験を行った。溶融したCsIの濡れ性を評価することで、固体の表面形態がCsIの溶融物性に与える影響を評価した。