[3I16] Solidification and Stabilization for Pu nitrate solution at TRP

4. Respond to equipment problems at PCDF

*SHINJI NUMATA1, HIDEMI ISOMAE1, MASAMI OHMURA1, KOICHI TSUTAGI1, DAISUKE KOBAYASHI1, DAISHI NAKAMURA1, MASAHIRO NEMOTO1, MASAYOSHI IIDA2, KAZUMA TAJIRI2, TSUTOMU KURITA1 (1. Japan Atomic Energy Agency, 2. E&E Techno Service)

Keywords:solidification and Stabilization, Plutonium Conversion Development Facility, Bellows, Vacuum Pipe

硝酸プルトニウム溶液(以下、「Pu溶液」という)の固化安定化処理の対応期間中、Pu転換施設の焙焼還元炉の伸縮継手及び溶液移送用の真空配管において発生した、不具合事象の対応について報告する。