V. Nuclear Fuel Cycle and Nuclear Materials » 501-1 Basic Properties/501-2 Nuclear Fuel and the Irradiation Behavior

[1A07-10] Reaction of Cesium with Stainless Steel

Mon. Mar 16, 2020 2:45 PM - 3:50 PM Room A (Lecture Bildg. L 1F L-4)

Chair:Kyoichi Morimoto(JAEA)

3:30 PM - 3:45 PM

[1A10] Wettability of liquid CsI on the SUS316 solid surface

*Hiroto Ishii1, Yuji Ohishi1, Hiroaki Muta1, Eriko Suzuki2, Kunihisa Nakajima2, Shuhei Miwa2, Masahiko Osaka2, Masayoshi Uno3, Ken Kurosaki3,4 (1. Osaka University, 2. Japan Atomic Energy Agency, 3. Research Institute of Nuclear Engineering, University of Fukui, 4. Institute for Integrated Radiation and Nuclear Science, Kyoto University)

Keywords:Wettability, CsI, SUS316, Fission products

原子炉構造材として使用されているSUS316固体表面における液体CsIの濡れ挙動を静滴法で評価した。