[2I1-30] Construction of a mixed entropy battery using the biphasic zwitterion salt-aqueous solution system showing LCST-type phase transition
01.Oral A
PC Setting Time : 13:00 - 13:10
Keywords:mixed entropy battery、zwittreion、lower critical solution temperature