14:15 〜 14:35
[S1.22] Characterization of FeCoNiMnV high entropy alloy fabricated by ball milling and spark plasma sintering
キーワード:High entropy alloy、Phase evolution、High strength alloy、Milling、Spark plasma sintering
Sintering temperature leads to the formation of tetragonal phases in addition to the FCC matrix.The maximum compressive strength of 1470 MPa is obtained for the sample tested at room temperature.