2017年第78回応用物理学会秋季学術講演会

講演情報

一般セッション(ポスター講演)

4 JSAP-OSA Joint Symposia 2017 » 4 JSAP-OSA Joint Symposia 2017 (poster)

[8a-PB2-1~11] 4 JSAP-OSA Joint Symposia 2017 (poster)

2017年9月8日(金) 09:30 〜 11:30 PB2 (国際センター2F)

09:30 〜 11:30

[8a-PB2-5] Terpolymer-based polymer optical fiber for multimodal polarization-maintaining

Daichi Mizorogi1、Eisuke Nihei2、Rei Furukawa1 (1.UEC、2.Keio Univ.)

キーワード:optical fiber, polymer, polarization-maintaining

Polarization-maintaining (PM) optical fiber is used in high-speed optical communication and fiber-optic interferometric sensing. Existing PM optical fiber that is known for PANDA fibers intentionally form a large birefringence in the core radially. By taking this structure, the PM function is obtained by suppressing the energy exchange between the orthogonal polarization components of the singlemode optical fiber. However, this principle is not effective in multimode fiber. In the past, it has been reported that a polymer optical fiber (POF) with its core fabricated using copolymer that can reduce intrinsic birefringence, namely, methyl methacrylate (MMA) and benzyl methacrylate (BzMA), exhibit a high extinction ratio compared to the other multimode optical fibers on the premise that no load is applied. Therefore, in this study, POF of ternary core including 2,2,2-trifluoroethyl methacrylate (3FMA) in addition to the earlier material pair was fabricated. P (MMA / 3 FMA / BzMA = 52.0 / 42.0 / 6.0 (w / w / w) is known to be effective in eliminating two types of birefringence, namely, photoelastic birefringence and orientational birefringence. As a result, it was proved that polarization maintaining effect is provided even when load is applied to this multimode fiber.