[15p-P3-20] Lattice expansion by post annealing of SrTiO3 films made by pulsed laser deposition using fourth harmonic Nd:YAG pulsed laser
Keywords:PLD, annealing effect, YAG
Poster presentation
6 Thin Films and Surfaces » 6.3 Oxide electronics
Wed. Mar 15, 2017 1:30 PM - 3:30 PM P3 (BP)