2:45 PM - 3:00 PM
△ [18p-B403-7] Growth of Large Bi-based High-Temperature Superconducting Whisker with High Jc
Keywords:Bi-based HTS, Wisker
Bi-based high-temperature superconducting whisker natively has very high Jc due to their strong pinning center caused by replacement of Sr site by Ca ion. However, the larger a replacement amount of Sr by Ca becomes, the smaller a size of whisker becomes. Therefore, it prevents Bi-based high-temperature superconducting whisker from being used in wider application field.
We focused on density increasing of alumina catalyst in the base material. Moreover, we try growth of large that Bi-based high-temperature superconducting whisker of high replacement amount of Sr by Ca.
We focused on density increasing of alumina catalyst in the base material. Moreover, we try growth of large that Bi-based high-temperature superconducting whisker of high replacement amount of Sr by Ca.