[15p-A202-6] Magnetic separation and enrichment of MnBi by solidification in a high magnetic field

keisuke suzuki1, Kensuke Nakazawa1, Isao Yamamoto1 (1.Yokohama Nat'l Univ.)

Keywords:magnetic separation, MnBi, magnetic fluid

Magnetic field effects on solidification in a high magnetic field has been reported in many studies. In this study, we focused on MnBi. A sample which has a composition having the same Curie temperature Tc and melting point Tm was solidified in magnetic field to enrich and separate MnBi components.The Mn10Bi90 alloy prepared by arc melting method from 4N-Mn and 5N-Bi was vacuum sealed in a glass tube with a diameter of 8 mm. The alloy was heated up to 632 K for 0.5 h and then vertical magnetic field of up to 5 T was applied. The sample was cooled to 545 K of melting temperature of pure Bi with cooling rate of 0.5 K/min. Large MnBi grains were observed near and outside the sample center for the sample prepared in 3 T. The large grains were aligned direction of the magnetic field of 5 T, and small grains of about 150 μm were arranged in a rod shape. On the other hand, spikes were observed in the vicinity of the circumference of the sample to which 3 T was applied, suggesting the appearance of ferromagnetism in liquid state. The same spikes have been reported only in supercooled Co, however, this is the first observation in binary alloys.