11:30 AM - 11:45 AM
[1Da11] Rapid degradation of protein using gas-liquid interface plasma
In order to evaluate the performance of the decomposition rate of gas-liquid interface plasma for the decomposition of polymers, we decomposed proteins known as persistent polymers. We have compared our data with those by the reported method of microbubble-assisted plasma in water. In the case of microbubble-assisted plasma in water, it tooks 60 minutes for reducing 0.1 mg / mL down to 0.01 mg / L or less, whereas in the case of our method, it tooks only 3 minutes.