[P055C] Selective depression of Pb-activated sphalerite with oxalic acid in sphalerite-galena flotation System

○Eladl Doaa1、 Suyantara Gde Pandhe Wisnu1、 Miki Hajime1、Naoko Okibe1 (1. Kyushu University)

キーワード:Organic acid、Green flotation、Pb2+activated sphalerite、Pb-Zn separation、Oxalic acid

Galena (PbS) and sphalerite (ZnS) often coexist in sulfide mineral ores. Flotation is commonly used to separate these minerals, but depressing ZnS in the flotation process can be challenging, particularly when ZnS is activated by Pb2+ ions dissolved from Pb bearing minerals. In this study, oxalic acid was used as a selective, efficient, and environmentally friendly depressant to separate PbS from Pb2+-activated ZnS. Micro-flotation experiments, FTIR, and XPS analysis were conducted to investigate the depressant mechanism of oxalic acid. Single-mineral flotation results showed that sphalerite was selectively depressed in the presence of oxalic acid with a mineral recovery of 20 %. In addition, the mixed mineral flotation recoveries of PbS and ZnS were 83% and 17 %, respectively. This effect is attributed to the precipitation of Pb oxalate on the surface of ZnS, causing a change in its hydrophobic properties. Conversely, Pb oxalate precipitationon the PbS surface resulted in a significant increase in flotation recovery. The results indicate that the use of oxalic acid as a depressant allows for the selective flotation of Pb-activated ZnS, effectively separating it from PbS.