2017 Fall Meeting

Presentation information

Oral presentation

IV. Nuclear Fuel Cycle and Nuclear Materials » 402-1 Nuclear Materials and the Irradiation Behavior

[2I08-17] SiC

Thu. Sep 14, 2017 2:45 PM - 5:25 PM Room I (C310 - C Block)

Chair:Hirotatsu Kishimoto (Muroran Inst. of Tech.)

5:00 PM - 5:15 PM

[2I17] Role of irradiation defects in SiC on hydrothermal corrosion

*Sosuke Kondo1, Yuki Maeda2, Kazuhiro Fukami2, Tatsuya Hinoki1 (1. Institute of Advanced Energy, Kyoto University, 2. Department of Materials Science and Engineering, Kyoto University)

Keywords:Silicon Carbide, corrosion, semiconductor, irradiation defect

高温高圧水中でのSiCの腐食に及ぼす照射欠陥の影響を、イオン、電子線照射した高純度SiCを対象とした電気化学挙動および材料中の欠陥準位の相関評価により検討した成果を発表する。