2019 Annual Meeting

Presentation information

Oral presentation

V. Nuclear Fuel Cycle and Nuclear Materials » 503-1 Reactor Chemistry, Radiation Chemistry, Corrosion, Water Chemistry,Water Quality Control

[2D01-06] Corrosion Chemistry 2

Thu. Mar 21, 2019 10:15 AM - 11:55 AM Room D (Common Education Bildg. 2 1F No.12)

Chair:Yusa Muroya(Osaka Univ.)

10:15 AM - 10:30 AM

[2D01] Study of the accelerated corrosion of carbon steel in air-solution alternating condition

(1)Effect of the concentration of diluted seawater

*Takashi Tsukada1, Kyohei Otani1, Hiroshi Terakado1, koei ebata1, Fumiyoshi Ueno1 (1. Japan Atomic Energy Agency)

Keywords:rotating-type corrosion test, carbon steel, diluted seawater, primary containment vessel

As reported previously, corrosion behavior of carbon steel in the artificial diluted seawater has been examined by the rotating-type corrosion test method and the corrosion rate was accelerated from 3-5 times by the air-solution alternating condition. In this study, an effect of the concentration of diluted seawater at 30ºC will be presented.