The 81st JSAP Autumn Meeting, 2020

Presentation information

Oral presentation

9 Applied Materials Science » 9.1 Dielectrics, ferroelectrics

[10a-Z26-1~8] 9.1 Dielectrics, ferroelectrics

Thu. Sep 10, 2020 8:30 AM - 10:45 AM Z26

Shintaro Ueno(Univ. of Yamanashi), Takaaki Morimoto(National Defence Academy)

10:15 AM - 10:30 AM

[10a-Z26-7] High temperature alternating current poling for 0.24Pb(In1/2Nb1/2)O3-0.46Pb(Mg1/3Nb2/3)O3-0.30PbTiO3 single crystals

〇(M2C)Cong Luo1,2, Yiqin Sun2, Tomoaki Karaki2, Yohachi Yamashita2, Jiayue Xu1 (1.Shanghai Inst. Tech., 2.Toyama Pref. Univ.)

Keywords:high temperature, alternating current poling, PIMN-0.30PT

Recently, an increasing number of researchers have focused on Pb(In1/2Nb1/2)O3-Pb(Mg1/3Nb2/3)-PbTiO3 (PIN-PMN-PT) ternary system single crystal (SC) possessing higher phase change temperature (Tpc) > 90 oC, which can be used in wider temperature range comparing with traditional PMN-xPT binary system SC. In this work, we have investigated high temperature alternate current poling (ACP) on [001] oriented 0.24PIN-0.46PMN-0.30PT (PIMN-0.30PT) SC manufactured by continuous-feeding Bridgman (CF BM) method which can partly eliminate the compositional segregation compared with the traditional one charge Bridgman method. High dielectric permittivity (εT330) of 6730 and piezoelectric constant d33 of 2240 pC/N, which were both 24% larger than those of direct current poling (DCP) using same poling voltage, was obtained by the ACP condition of 4 kVrms/cm, 10 Hz, and 12 cycles at 90 oC. Temperature dependence of these εT330 (Fig. 1) and phase analysis by X-ray diffraction (XRD) (Fig. 2) of these ACP and DCP SCs showed clear different properties. We concluded that the best ACP poling temperature for CF BM PIMN-0.30PT SC is 90 oC which is almost as same as its Tpc.