9:30 AM - 11:30 AM
[22a-P4-13] The infrared bolometer element using the ZnO / Pt barrier
Keywords:Infrared bolometer,ZnO,Temperature coefficient of resistance
Poster presentation
6 Thin Films and Surfaces » 6.3 Oxide electronics
Tue. Mar 22, 2016 9:30 AM - 11:30 AM P4 (Gymnasium)