The 60th JSAP Spring Meeting,2013

Presentation information

Regular sessions(Poster presentation)

21. Joint Session K » 21.1 Joint Session K "Wide bandgap oxide semiconductor materials and devices"

[27a-PB4-1~25] 21.1 Joint Session K "Wide bandgap oxide semiconductor materials and devices"

Wed. Mar 27, 2013 9:30 AM - 11:30 AM PB4 (2nd gymnasium)

[27a-PB4-18] Thick film growth of zinc oxide on n-type GaN by electrodeposition

Mitsuteru Sainokami1, Junpei Ikegami1, Kazuyuki Uno1, Ichiro Tanaka1 (Wakayama Univ.1)

Keywords:酸化亜鉛、電気化学堆積法